RCI 20 ................... download or print pdf
DESCRIPTION:
RCI 20 Is a cured and hence more flexible version of RCI 20 which has been specially developed to allow customers the ability to undertake some degree of reradiusing andd cure out them selves.
To help the radiusing operation and to convert RCI 20 into RCI 21, the matrerial should firstly be warmed between 120ºC (248ºF) and 150ºC (302ºF) before gently inducing a change of radius. However, care should be taken whilst carrying out this procedure to ensure that no area is radiused more than another, otherwise cracking or possible distorion could occur.
Once the new radius has been achieved the material should be clamped on both the inner and outer surfaces between metal formers and cured at a temperature of 200ºC to 230ºC (392ºF to 446ºF) for a minimum of one hour, before being allowed to cool to approximately 100ºC (212 ºF) and the formers removed.
This data sheet should be read in conjunction with the data sheet for RCI 21.
........................................................................ Top